Specification for low nickel-chromium steel (bar for the manufacture of forged bolts only)
|
|
|
На языке оригинала
|
Пишите на gost@gostinfo.ru
|
|
|
|
Specification for chromium-molybdenum-vanadium-niobium heat-resisting steel billets, bars, forgings and parts (930-1080 MPa) (Cr 10.5, Mo 0.6, V 0.2, Nb 0.3)
|
|
|
На языке оригинала
|
Пишите на gost@gostinfo.ru
|
|
|
|
Specification for chromium-nickel-molybdenum-vanadium heat-resisting steel billets, bars, forgings and parts (930-1130 MPa: limiting ruling section 150 mm) (Cr 12, Ni 2.5, Mo 1.7, V 0.3)
|
|
|
На языке оригинала
|
Пишите на gost@gostinfo.ru
|
|
|
|
Specification for chromium-cobalt-molybdenum-vanadium-niobium heat-resisting steel billets, bars, forgings and parts (consumable electrode remelted) (1000-1140 MPa) (Cr 10.5, Co 6, Mo 0.8, V 0.2, Nb 0.3)
|
|
|
На языке оригинала
|
Пишите на gost@gostinfo.ru
|
|
|
|
Specification. 2% nickel-chromium-molybdenum steel billets, bars, forgings and parts (1230-1430 MPa: limiting ruling section 40 mm)
|
|
|
На языке оригинала
|
Пишите на gost@gostinfo.ru
|
|
|
|
Specification. 2% nickel-chromium-molybdenum steel billets, bars, forgings and parts (880-1080 MPa: limiting ruling section 150 mm)
|
|
|
На языке оригинала
|
Пишите на gost@gostinfo.ru
|
|
|
|
Specification for nickel-silicon-chromium-molybdenum-vanadium steel (vacuum arc remelted) billets, bars, forgings and parts (1900-2100 MPa: limiting ruling section 75 mm)
|
|
|
На языке оригинала
|
Пишите на gost@gostinfo.ru
|
|
|
|
Specification for 4% nickel-chromium-molybdenum case-hardening steel (vacuum arc remelted) billets, bars, forgings and parts (1320-1520 MPa)
|
|
|
На языке оригинала
|
Пишите на gost@gostinfo.ru
|
|
|
|
Specification. 3% nickel-chromium-molybdenum case-hardening steel billets, bars, forgings and parts (1180-1380 MPa)
|
|
|
На языке оригинала
|
Пишите на gost@gostinfo.ru
|
|
|
|
Specification for 1% chromium-molybdenum steel bars for the manufacture of forged bolts and forged nuts
|
|
|
На языке оригинала
|
Пишите на gost@gostinfo.ru
|
|
|
|
Specification for 12% chromium-nickel-molybdenum-vanadium heat-resisting steel bars for the manufacture of fasteners (1100-1300 MPa: limiting ruling section 50 mm)
|
|
|
На языке оригинала
|
Пишите на gost@gostinfo.ru
|
|
|
|
Specification for chromium-nickel corrosion-resisting steel - bright bars and parts (540 MPa, limiting ruling section 160 mm) (Cr 18, Ni 10.5, controlled nitrogen content)
|
|
|
На языке оригинала
|
Пишите на gost@gostinfo.ru
|
|
|
|
Specification for chromium-nickel-molybdenum corrosion-resisting steel. Bright bars and parts (540 MPa, limiting ruling section 160 mm) (Cr 17.5, Ni 12.5, Mo 2.25, controlled nitrogen content)
|
|
|
На языке оригинала
|
Пишите на gost@gostinfo.ru
|
|
|
|
Specification for 18% nickel-cobalt-molybdenum maraging steel forging stock, forgings, bars and parts (1800 MPa: double vaccuum melted)
|
|
|
На языке оригинала
|
Пишите на gost@gostinfo.ru
|
|
|
|
Specification for nickel-chromium-molybdenum-vanadium steel forging stock, forgings, bars and parts (1900 MPa:limiting ruling section 100 mm)
|
|
|
На языке оригинала
|
Пишите на gost@gostinfo.ru
|
|
|
|
1 % Chromium-molybdenum steel billets, bars, forgings and parts. (1150 to 1300 MPa: Limiting ruling section 16 mm) (Suitable for welding)
|
|
|
На языке оригинала
|
Пишите на gost@gostinfo.ru
|
|
|
|
Chromium-nickel-aluminium corrosion resisting steel (precipitation hardening) rod, cold drawn wire and springs
|
|
|
На языке оригинала
|
Пишите на gost@gostinfo.ru
|
|
|
|
Specification for cold-rolled 18/10 chromium-nickel corrosion-resisting steel sheet and strip (titanium stabilized: 800MPa)
|
|
|
На языке оригинала
|
Пишите на gost@gostinfo.ru
|
|
|
|
Specification for cold-rolled 18/10 chromium-nickel corrosion-resisting steel sheet and strip (niobium stabilized: 800 MPa)
|
|
|
На языке оригинала
|
Пишите на gost@gostinfo.ru
|
|
|
|
Specification for softened 18/10 chromium-nickel corrosion-resisting steel sheet and strip (titanium stabilized: 540 MPa)
|
|
|